上海耀澄贸易有限公司
主营产品:
2023年07月24日 14:59
牌号 |
ETFE2185 |
类型 |
其他 |
用途级别 |
挤出级 |
厂家(产地) |
日本杜邦 |
DuPont Tefzel® HT-2185
Product Information
screw injection molding machines are preferred.
Corrosion-resistant metals should be used in contact
with molten resin. Extruder barrels should be long,
relative to diameter, to provide residence time for
heating the resin to approximately 340°C (640°F).
Safety Precautions
WARNING!
VAPORS CAN BE LIBERATED THAT MAY
BE HAZARDOUS IF INHALED.
Before using Tefzel® HT-2185, read the Material Safety
Data Sheet and the detailed information in the “Guide
to the Safe Handling of Fluoropolymer Resins,” latest
edition, published by the Fluoropolymers Division of
The Society of the Plastics Industry—available from
DuPont.
Open and use containers only in well-ventilated areas
using local exhaust ventilation (LEV). Vapors and
fumes liberated during hot processing, or from smoking
tobacco or cigarettes contaminated with Tefzel®
HT-2185, may cause flu-like symptoms (chills, fever,
sore throat) that may not occur until several hours after
exposure and that typically pass within about 24 hours.
Vapors and fumes liberated during hot processing
should be exhausted completely from the work area;
contamination of tobacco with polymers should be
avoided.
Mixtures with some finely pided metals, such
as magnesium or aluminum, can be flammable or
explosive under some conditions.
Storage and Handling
The properties of Tefzel® HT-2185 resins are not
affected by storage time. Ambient storage conditions
should be designed to avoid airborne contamination
and formation of water on the resin when it is removed
from containers.
Freight Classification
Tefzel® when shipped by rail or express is classified
“Plastics, Synthetic, O.T.L., NOIBN.” Resin shipped
by truck is classified “Plastics, Materials O.T.F.C.E.
or S. Granules.”
Packaging
Tefzel® fluoropolymer resins are packaged 20.3 kg (45-lb)
multilayer, kraft bags with an integral polyethylene liner.
联系方式